全国服务热线 TEL

0758-8417888
  • 环氧金磨石自流平中涂
  • 环氧金磨石自流平中涂

环氧金磨石自流平中涂

  • 系列:地坪漆
  • 名称:环氧金磨石自流平中涂
  • 规格:20L
  • 颜色:白芝麻、芝麻灰、北欧白、爵士灰、浅灰、大红色、奶酪色、星辰黄、简约白、奶油白、可可蛋奶、琥珀色、杏子灰、浅灰色、碳灰、冰蓝灰、北欧蓝、雪蓝、翡翠绿、清新绿
  • 特点:

产品详情

一、作用

找平地面、填补坑洞缝隙、增加地坪厚度与抗压耐磨,衔接底漆和面漆。

1. Functions

Levels the floor surface, fills holes and cracks, increases overall floor thickness, enhances compressive strength and wear resistance, and provides a bonding bridge between the primer and the topcoat.

二、配比

AB按10:1(重量)

又或者会要“配比比列见标签”这句话也翻译

2. Mixing Ratio

Mix A and B at a ratio of 10:1 by weight.

The exact mixing ratio is shown on the product label.

三、施工条件

气温10-35℃,地面干燥无尘,底漆干透8小时以上再施工。

3. Application Conditions

Ambient temperature: 10-35℃

Substrate must be dry and dust-free.

The primer coat must be fully dry at least 8 hours before applying this intermediate coat.

四、施工流程 

1. 地面清理干净,裂缝先用补缝胶修补

2. 按比例称重搅拌均匀,

3. 批刮/镘刀摊铺找平,抹平高低差

4. 常温12小时干透,即可打磨除尘上面漆

4. Application Procedure

1. Clean the floor surface thoroughly. Pre-fill any cracks with a suitable crack-repair compound.

2. Weigh the components according to the specified ratio and mix thoroughly until uniform.

3. Apply the material using a trowel or screed, spreading evenly to level the surface and smooth out any height differences.

4. At room temperature, allow the coat to dry for 12 hours. After that, it can be sanded, dusted, and the topcoat can be applied.

五、参数参考

用量0.6-0.8kg/㎡,24小时轻载,7天完全固化。

5. Reference Data

Coverage: 0.6-0.8kg/m².

Light foot traffic allowed after 24 hours.

Full cure achieved after 7 days.

六、安全存放 

阴凉密封保存,保质期12个月;施工通风,佩戴防护用品,远离明火,工具用专用稀释剂清洗。

6. Storage and Safety

Store in a cool, dry place in sealed containers. 

Shelf life: 12 months.

Ensure adequate ventilation during application. 

Wear gloves and safety goggles. 

Keep away from open flames.

Clean tools with the designated thinner before the material cures.

七、常见问题 

1. 起壳:底漆未干、地面粉尘未清

2. 不干:配比不对、搅拌不均匀

3. 开裂:涂层过厚、基层未加固

7. Troubleshooting

1. Delamination / lifting       Primer not fully cured; dust or dirt remaining on the substrate.

2. Incomplete curing / tackiness     Incorrect mixing ratio; insufficient stirring.

3. Cracking                 Excessive film thickness; insufficient substrate reinforcement.